Thermocouple sheaths. Ethylene dichloride (EDC) cracking tubes.

Rated 4.9/5 based on 222 customer reviews
Share:
Content

Nickel Alloy 600 and Inconel? 600 are readily fabricated (hot or cold) and can be joined using standard welding, brazing, and soldering processes.Hot working should be performed between 1600¡ã F and 2250¡ã F avoiding any work between1200-1600¡ã F because the ductility decreases in this temperature range.Machining is somewhat comparable to 304 and requires heavy duty tooling to handle this material, and it can be cold formed with standard fabrication techniques.