Alloy C263 is an aluminum-titanium age hardening nickel base superalloy welding wire. Gas tungsten arc welding is normally carried out using argon shielding gas. Argon +5% hydrogen has been used. Alloy C263 base metal is normally welded in the annealed condition 2100° F, rapid cool). After welding, the assembly may be aged 8 hours at 1470° F, air cool. Repair welding of alloy C263 components may be done in the age hardened condition.
Chemistry
|
Cr
|
Ni
|
Mo
|
Co
|
Al
|
Ti
|
Al+Ti
|
B
|
C
|
Fe
|
Mn
|
Si
|
P
|
S
|
Ag
|
Bi
|
Pb
|
Cu
|
MIN
|
19
|
-
|
5.6
|
19.0
|
0.3
|
1.9
|
2.4
|
-
|
0.01
|
-
|
-
|
-
|
-
|
-
|
-
|
-
|
-
|
-
|
MAX
|
21.00
|
Balance
|
6.10
|
21.00
|
0.60
|
2.40
|
2.80
|
0.005
|
0.08
|
0.70
|
0.60
|
0.40
|
0.015
|
0.007
|
0.0005
|
0.0001
|
0.002
|
0.20
|
Specifications
AMS 5872, AMS 5872E, AMS 5886, AMS 5966
EN 2.4650
GE B50A771, GE B50A783
RR 9500/16
UNS N07263
Werkstoff 2.4650
Inventory
C263 Plate, C263 Round Bar, C263 Sheet, C263 Weld Wire
Common Trade Names
Cobalt 263, Nimonic® Alloy C263
Features
• High strength as age-hardened
Applications
• Welding 263 base metal
• Welding GTD222 investment castings
Physical Properties
Density: 0.302 lb/in3
Melting Range: 2372-2471° F
Temperature, ° F
|
400
|
800
|
1000
|
1200
|
1400
|
1600
|
1800
|
Coefficient* of Thermal Expansion,
in/in° F x 10-6
|
6.7
|
7.4
|
7.7
|
8.1
|
8.7
|
9.6
|
10.2
|
* 70° F to indicated temperature.
Nimonic®