Best price incoloy 800 1.4876 NO8800 plate Hot Rolled sheet coil
1.ASTM Specification Of Incoloy 800 Plate:
Alloy
|
Sheet/Plate
|
Alloy 800 (UNS N08800) |
B409 |
Alloy 800H (UNS N08810) |
B409 |
Alloy 800HT (UNS N08811) |
B409 |
2.Incoloy800 (UNS NO8800/W.Nr.1.4876/X10NiCrAlTi3220) CHEMICAL COMPOSITION
% |
C |
Mn |
Si |
S |
P |
Cu |
B |
Fe |
Min |
|
|
|
|
|
|
|
Bal |
Max |
0.01 |
1.5 |
1 |
0.015 |
|
0.75 |
|
% |
V |
Mo |
Nb |
Cr |
Ni |
Al |
Ti |
|
Min |
|
|
|
19 |
30 |
0.15 |
0.15 |
|
Max |
|
|
|
23 |
35 |
0.6 |
0.6 |
|
3.Incoloy800 (UNS NO8800/W.Nr.1.4876/X10NiCrAlTi3220) Heat treatment
Bar、Hot rolled plate,cold rolled plate,seamless tube、cold rolled strip and forging:1000℃-1060℃,Air cool
4.Incoloy800 (UNS NO8800/W.Nr.1.4876/X10NiCrAlTi3220) MECHANICAL PROPERTIES
Density |
Melting |
Heat treatment |
Tensile strength |
Yield strength |
Elongation |
Reduction of area |
Brinell Hardness |
g/cm3 |
℃ |
σb/MPa |
σp0.2/MPa |
σ5 /% |
φ/ % |
HBS |
7.94 |
1357 |
Solution treatment |
≥480 |
≥170 |
≥35 |
|
|
1385 |
Incoloy800 (UNS NO8800/W.Nr.1.4876/X10NiCrAlTi3220) Spec.NO.
Bar\Forging:ASTM B164、ASTM B564
Cold\rolled plate:ASTM B127
Tube:ASTM B163
5.Mechanical & Physical Properties :
Density |
Melting Point |
Tensile Strength |
Yield Strength (0.2%Offset) |
Elongation |
7.94 g/cm3 |
1385 °C (2525 °F) |
Psi – 75,000, MPa – 520 |
Psi – 30,000, MPa –205 |
30 % |
6.Specifications and Designations
STANDARD |
UNS |
WERKSTOFF NR. |
EN |
AFNOR |
JIS |
GOST |
BS |
OR |
Incoloy 800 |
N08800 |
1.4876 |
X10NiCrAlTi32-20 |
Z8NC32-21 |
NCF 800 |
ЭИ670 |
NA 15 |
XH32T |
Incoloy 800H |
N08810 |
1.4958 / 1.4876 |
X5NiCrAlTi31-20 |
Z8NC33-21 |
NCF 800H |
ЭИ670 |
NA 15(H) |
XH32T |
Incoloy 800HT |
N08811 |
1.4859 / 1.4876 |
X8NiCrAlTi32-21 |
- |
NCF 800HT |
ЭИ670 |
NA 15(HT) |